Re: board thickness



with two boards, yes, with three cross laminate for extra strength, but I
would have the outers running parallel to the spine and the center
perpendicular.

p.


~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

Peter Verheyen, Listowner: Book_Arts-L
mailto:pdverhey@dreamscape.com
http://www.dreamscape.com/pdverhey


On Thu, 21 Jan 1999, Joanna Perry wrote:

> Dear Peter, please excuse these questions if they are foolish. You mentioned
> laminating 2 ply matt board to get thicker board. Should the grain go the
> same way on both pieces?  If so, does the grain go with the spine?
>